Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0492 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0492 lb/in³
Garlock MULTI-SWELLâ„¢ 3760 Compressed Aramid Fiber Gasketing
Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregul..
Density 1.36 g/cc
0.0492 lb/in³
Garlock MULTI-SWELLâ„¢ 3760-U Compressed Aramid Fiber Gasketing
Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregul..
Density 1.36 g/cc
0.0492 lb/in³
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material
THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u..
Density 1.36 g/cc
0.0492 lb/in³
Garlock THERMA-PURâ„¢ 4122-KAMM High Temperature Gasketing Material
THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u..
Density 1.36 g/cc
0.0492 lb/in³
Wet
Unifrax Fiberfrax® LDS Moldable Moldable Insulation
Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b..
Density 1.36 g/cc
0.0492 lb/in³
Wet
Unifrax Fiberfrax® Pumpable-LDS Pumpable Insulation
Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have te..
Density 1.36 g/cc
0.0492 lb/in³
BNZ Materials CS85 High Temperature Structural Insulation
NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,..
Density 1.36 g/cc
0.0492 lb/in³
Garlock THERMA-PUR™ 4122-FC High Temperature Gasketing Material
THERMa-PUR™ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a uniqu..
Copyright © lookpolymers.com All Rights Reserved