Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.361 g/cc
0.04917 lb/in³
JIS-Z-8807
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.63 MPa
5748 psi
JIS-K-6740
Elongation at Break 84 %
84 %
JIS-K-6740
Flexural Strength 59.0 MPa
8560 psi
JIS-K-6740
Flexural Modulus 2.41 GPa
350 ksi
JIS-K-6740
Izod Impact, Notched 1.8639 J/cm

@Temperature -20.0 °C
3.4918 ft-lb/in

@Temperature -4.00 °F
JIS-K-6740
4.2183 J/cm

@Temperature 0.000 °C
7.9026 ft-lb/in

@Temperature 32.0 °F
JIS-K-6740
11.97 J/cm

@Temperature 23.0 °C
22.42 ft-lb/in

@Temperature 73.4 °F
JIS-K-6740
Penetration 76
76
[°C], penetration temperature; JIS-K-6740
Thermal Properties Metric English Comments
Vicat Softening Point 89.0 °C
192 °F
JIS-K-6740
Descriptive Properties Value Comments
Thermostability, min, JIS-K-6723 60