Physical Properties Metric English Comments
Density 0.988 g/cc
0.0357 lb/in³
ASTM D792
Mytex Polymers AS78L(W)-GM-02 Polypropylene, Rubber modified, Compounded
Description: AS78L(W)-GM-02 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties.Key Applications: Bumper fascias and all other exterior partsInform..
Density 0.989 g/cc

@Temperature 20.0 °C
0.0357 lb/in³

@Temperature 68.0 °F
LyondellBasell Glycol Ether DE Diethylene glycol ethyl ether
Information provided by Lyondell.
Density 0.989 - 1.04 g/cc
0.0357 - 0.0376 lb/in³
309-2D Hardener
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive
Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh..
Density 0.989 g/cc
0.0357 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati..
Density 0.987 g/cc

@Temperature 25.0 °C
0.0357 lb/in³

@Temperature 77.0 °F
BASF PolyTHF® 650 Polyether
Description: PolyTHF 650 is a colorless, odorless waxy substance. It is sparingly soluble in water and soluble organic solvents.Applications: Intermediate used in the production of: Synthesis of ela..
Density 0.988 g/cc
0.0357 lb/in³
BASF 2-Ethylhexyl Choroformate
Formula: C9H17ClO2CAS: 24468-16-1Description: 2-Ethylhexyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyzes in the presence of water.Synonyms: Chloroformic acid 2..
Density 0.987 g/cc
0.0357 lb/in³
ASTM D792
Multibase Multi-Flam™ 1502 PP Black Polypropylene
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase