Mytex Polymers AS78L(W)-GM-02 Polypropylene, Rubber modified, Compounded

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Mytex Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS78L(W)-GM-02 Polypropylene, Rubber modified, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: AS78L(W)-GM-02 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties.Key Applications: Bumper fascias and all other exterior partsInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.988 g/cc
0.0357 lb/in³
ASTM D792
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Ash 14 %
14 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
15 sec; ISO 868
Tensile Strength, Yield 17.0 MPa
2470 psi
50 mm/min; ISO 527
Flexural Modulus 1.07 GPa
155 ksi
Chord; 2 mm/min; ISO 178
Izod Impact, Notched (ISO) 50.0 kJ/m²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ISO 75-1
Users viewing this material also viewed the following: