Physical Properties Metric English Comments
Density 0.761 g/cc
0.0275 lb/in³
Reade Advanced Materials Bentonite Powder (BaTiSi3O9)
Description: A rock composed essentially of a crystalline clay-like mineral formed by devitrification and the accompanying chemical alteration of a glassy igneous material, usually a tuff or volcani..
Density 0.760 g/cc
0.0275 lb/in³
Zircar Refractory Composites ZIRCAL-45 Refractory Board
Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com..
Density 0.760 g/cc
0.0275 lb/in³
Calculated number using basis weight and thickness
DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Density 0.762 g/cc

@Temperature 15.0 °C
0.0275 lb/in³

@Temperature 59.0 °F
ISO 12185
ExxonMobil Isopar™ K (EU) Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu..
Density 0.762 g/cc

@Temperature 15.6 °C
0.0275 lb/in³

@Temperature 60.0 °F
ASTM D4052
ExxonMobil Isopar™ K Naphtha Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation pr..
Density 0.762 g/cc

@Temperature 15.0 °C
0.0275 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Isopar™ L (AP) Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Asia PacificInformation pro..
Density 0.760 g/cc
0.0275 lb/in³
BASF Dibutylamine
Formula: C3H10N2CAS: 111-92-2Description: Dibutylamine is a clear colorless liquid with an amine-like odor.Synonyms: N,N-Di-n-butylamin, N-Butyl-1-butanamine, Di-N-ButylamineApplications: Intermedia..
Density 0.760 g/cc
0.0275 lb/in³
3M CC-2 Cable Cleaning Preparation Kits
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Density 0.760 g/cc
0.0275 lb/in³
blow pressure of 2 Bar; 20% density reduction
Akzo Nobel Blow Molding of HDPE with 3.25 % Expancel
Density 0.760 g/cc
0.0275 lb/in³
BASF Tripropylamine
Formula: C9H21NCAS: 102-69-2Description: Tripropylamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: Propyldi-n-propylamine, Tri-n-propylamine, N,N-Di..
Density 0.760 g/cc
0.0275 lb/in³
3M CC-3 Cleaning Pad Kits
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Density 0.760 g/cc
0.0275 lb/in³
3M CC-4 Cleaning Solvent
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Density 0.762 g/cc
0.0275 lb/in³
BASF tert.-Butyl Vinyl Ether
Formula: C6H12OCAS: 926-02-3Description: Tert.-Butyl vinyl ether is a colorless to yellow liquid, with an ether-like odor. It is sparingly soluble in water.Synonyms: 2(Ethenyloxy)-2-methylpropane, ..