DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard

Category Polymer , Thermoplastic , Nylon , Nylon, Aromatic
Manufacturer DuPont
Trade Name Nomex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications include 3-dimensional parts such as V-rings, angle rings and spools, as well as barrier, gap spacers and core tubes.Information provided by DuPont
Physical Properties Metric English Comments
Density 0.760 g/cc
0.0275 lb/in³
Calculated number using basis weight and thickness
Thickness 2000 microns
78.7 mil
ASTM D374, method D, using 17 N/cm²
Linear Mold Shrinkage 0.0070 cm/cm

@Temperature 105 °C
0.0070 in/in

@Temperature 221 °F
ASTM D3392
0.011 cm/cm

@Temperature 240 °C
0.011 in/in

@Temperature 464 °F
ASTM D3392
Linear Mold Shrinkage, Transverse 0.011 cm/cm

@Temperature 105 °C
0.011 in/in

@Temperature 221 °F
ASTM D3392
0.020 cm/cm

@Temperature 240 °C
0.020 in/in

@Temperature 464 °F
ASTM D3392
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 47.5 MPa
6890 psi
ASTM D828
Film Tensile Strength at Yield, TD 34.4 MPa
4990 psi
ASTM D828
Film Elongation at Yield, MD 13.8 %
13.8 %
ASTM D828
Film Elongation at Yield, TD 14.1 %
14.1 %
ASTM D828
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm
508 kV/in
AC rapid rise in air; ASTM D149
Descriptive Properties Value Comments
Basis Weight (g/m²) ASTM D3392