Physical Properties Metric English Comments
Density 0.640 g/cc
0.0231 lb/in³
Pyrotek A-2 Fiberglass Rope
An A-1 substitute fiberglass rope.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrotek.
Density 0.640 g/cc
0.0231 lb/in³
Pyrotek Pyrocast L-30 Moldable Refractory
Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommen..
Density 0.640 g/cc
0.0231 lb/in³
ASTM D3574A
Mearthane Durethaneâ„¢ F DF-225A Closed Cell Foam Polyurethane
TDI backbone: ester.Shore 00 Hardness: 70Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Density 0.640 g/cc
0.0231 lb/in³
ASTM D3574A
Mearthane Durethaneâ„¢ F DF-640A Closed Cell Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Density 0.640 g/cc
0.0231 lb/in³
ASTM D3574A
Mearthane Durethaneâ„¢ M DM-640A Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
Density 0.640 - 0.700 g/cc
0.0231 - 0.0253 lb/in³
Apparent
Gouda Vuurvast GI 23 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Density 0.640 g/cc
0.0231 lb/in³
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech..
Density 0.640 g/cc
0.0231 lb/in³
Available in multiple densities from manufacturer
Thermal Ceramics Cerafelt
Cerafelt products are lightweight, flexible refractory fiber insulators formed from exceptionally pure refractory oxides and bonded with an organic binder.These products are recommended for a wide r..
Density 0.640 g/cc
0.0231 lb/in³
Zircar Ceramics NKO Castertip
Main stay "low mass hard tip" used on all makes of continuous thin strip aluminum casting equipment. NKO is a rigid combination of refractory ceramic fiber and inorganic binders. Information provid..
Density 0.640 g/cc
0.0231 lb/in³
Zircar Refractory Composites RS-SI SILICA MOLDABLE
ZIRCAR Silica Moldable Type RS-SI Moldable is a wet blanket that is a combination of high purity amorphous silica fibers and inorganic silica binder. The fibers are 6-9 um in diameter and are consid..
Density 0.640 g/cc
0.0231 lb/in³
ASTM D792
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Density 0.640 g/cc
0.0231 lb/in³
ASTM D792
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Density 0.640 g/cc
0.0231 lb/in³
ASTM D792
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Density 0.640 g/cc
0.0231 lb/in³
helium pycnometer
CRG Industries Advantic™ 40 Syntactic Foam
Advantic is a series of lightweight, engineered foams consisting of manufactured glass, polymer, or ceramic hollow spheres embedded in a resin matrix, such as epoxy or cyanate ester. CRG Industries’..
Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
CMT Materials HYTAC® B1X High Durability Thermoplastic Syntactic
HYTAC-B1X is the first plug assist material to combine the toughness of an engineered thermoplastic with the low thermal conductivity of syntactic foam. Plug assist made from HYTAC-B1X will resist ..
Density 0.640 g/cc
0.0231 lb/in³
3M Bumpon™ SJ5208 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Density 0.640 g/cc
0.0231 lb/in³
3M Bumpon™ SJ5216 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Density 0.640 g/cc
0.0231 lb/in³
3M Bumpon™ SJ5904 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Density 0.640 g/cc
0.0231 lb/in³
3M Bumpon™ SJ5908 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Density 0.640 g/cc
0.0231 lb/in³
3M SJ5201 Protective Product, Die Cut Shapes
3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari..
Density 0.640 g/cc
0.0231 lb/in³
3M Bumpon™ SJ5916 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Density 0.640 g/cc
0.0231 lb/in³
3M SJ5202 Protective Product, Die Cut Shapes
3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari..