Pyrotek A-2 Fiberglass Rope

Category Ceramic , Glass
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek A-2 Fiberglass Rope.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An A-1 substitute fiberglass rope.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.640 g/cc
0.0231 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 540 °C
1000 °F