Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.280 g/cc | 0.0101 lb/in³ | Effective density of spheres |
Potters Industries Q-Cel® 6028 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | Ni Foam Starting Material |
FiberNide Nickel Aluminide Foam Atomic 10% Aluminum Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f.. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | Ni Foam Starting Material |
FiberNide Nickel Aluminide Foam Atomic 15% Aluminum Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f.. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | Ni Foam Starting Material |
FiberNide Nickel Aluminide Foam Atomic 20% Aluminum Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f.. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | Ni Foam Starting Material |
FiberNide Nickel Aluminide Foam Atomic 22% Aluminum Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f.. |
|||
Density | 0.280 - 0.600 g/cc | 0.0101 - 0.0217 lb/in³ | |
FiberNide Nickel Foam Description: Produced in one meter wide continuous sheets in thickness from 1.6 to 2 mm and sold in rolls. Principally used to make the positive plate in nickel metal hydride batteries.Information .. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | |
Unifrax Excelfrax® 1900 Panel Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | |
Zircar Refractory Composites ZIRCAL-18 Refractory Board Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m.. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | |
Hexcel® HexWeb® HDC-660 - 3/16 - 17.5 (R2) Heavy Density Core Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with eit.. |
|||
Density | 0.280 g/cc | 0.0101 lb/in³ | |
Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher .. |
|||
Density | <= 0.280 g/cc | <= 0.0101 lb/in³ | DIN 53479 A |
BIW ASTM Class 2D0 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |