Physical Properties Metric English Comments
Density 0.350 g/cc
0.0126 lb/in³
Typical, 3M QCM 14.24.6
3M HGS3000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.350 - 0.410 g/cc
0.0126 - 0.0148 lb/in³
True, 3M QCM 14.24.6
3M HGS4000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.350 g/cc
0.0126 lb/in³
3M S35 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.350 - 0.410 g/cc
0.0126 - 0.0148 lb/in³
3M S38 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.350 - 0.410 g/cc
0.0126 - 0.0148 lb/in³
3M S38HS Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.350 - 0.410 g/cc
0.0126 - 0.0148 lb/in³
True, 3M QCM 14.24.6
3M HGS5000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.350 - 0.500 g/cc
0.0126 - 0.0181 lb/in³
DIN 53479 A
BIW ASTM Class 2D3 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...