Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.160 - 0.192 g/cc | 0.00578 - 0.00694 lb/in³ | |
Pyrotek C-1 Ceramic fiber paper C-1 Fiberseal paper is a highly uniform paper which assures equal thermal conductivity throughout the product.ApplicationsHigh temperature gaskets Liners Expansion joints Thermal barrier Seals Blast.. |
|||
Density | 0.160 - 0.200 g/cc | 0.00578 - 0.00723 lb/in³ | ASTM D792 |
Microcell Composite Company CELLAMP® M5130 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Sawbones Cellular Rigid Polyurethane Foam 10 pcf Density Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone .. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites RSPA-SOL2 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites RSPA-SOL3 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | Typical, 3M QCM 14.24.6 |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.160 - 0.192 g/cc | 0.00578 - 0.00694 lb/in³ | |
Pyrotek C-1 Fiber Seal Pre-cut Gasket A highly uniform ceramic fiber paper offering even thermal conductivity.Information provided by Pyrotek. |