Microcell Composite Company CELLAMP® M5130 Thermoplastic Foam

Category Polymer , Thermoplastic
Manufacturer Microcell Composite Company
Trade Name CELLAMP®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Microcell Composite Company CELLAMP® M5130 Thermoplastic Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high damping characteristics. It is comfortable to the touch and has contour form memory characteristics.Information provided by Microcell Composite Company
Physical Properties Metric English Comments
Density 0.160 - 0.200 g/cc
0.00578 - 0.00723 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 42 - 46
42 - 46
ASTM D2240
Tensile Strength, Yield 0.785 MPa
114 psi
ASTM D412
Elongation at Yield 200 %
200 %
ASTM D412
Tear Strength 1.96 kN/m
11.2 pli
ASTM D624
Compression Set 80 %

@Temperature 70.0 °C,
Time 21600 sec
80 %

@Temperature 158 °F,
Time 6.00 hour
50%; ASTM D395
Thermal Properties Metric English Comments
Shrinkage 2.0 %

@Temperature 70.0 °C,
Time 2400 sec
2.0 %

@Temperature 158 °F,
Time 0.667 hour
ASTM D1204
Descriptive Properties Value Comments
Resiliency (%) 30
ASTM D2632