| Category | Polymer , Thermoplastic , Fluoropolymer |
| Manufacturer | Zeus |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Zeus EFEP Tubing.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
| Water Absorption | <= 0.10 % | <= 0.10 % | ASTM D257 |
| Crystallinity | 10 % | 10 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 75 | 75 | ASTM D2240 |
| Tensile Strength, Ultimate | 40.0 - 50.0 MPa | 5800 - 7250 psi | ASTM D638 |
| Elongation at Break | 420 - 460 % | 420 - 460 % | ASTM D638 |
| Modulus of Elasticity | 0.490 - 0.780 GPa | 71.1 - 113 ksi | ASTM D638 |
| Flexural Modulus | 0.880 - 1.37 GPa | 128 - 199 ksi | ASTM D790 |
| Coefficient of Friction | 0.055 - 0.078 | 0.055 - 0.078 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 160 - 195 °C | 320 - 383 °F | |
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
| Decomposition Temperature | 350 °C | 662 °F | ASTM E1131 |
| Oxygen Index | 31 % | 31 % | ASTM D2863 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.338 - 1.34 | 1.338 - 1.34 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Dielectric Constant | 2.6 @Frequency 1.00e+6 Hz |
2.6 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |