Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Williams Advanced Alloys WS199 Solder

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS199 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 7.85 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
Thermal Properties Metric English Comments
CTE, linear 24.5 µm/m-°C

@Temperature 20.0 °C
13.6 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 59.0 W/m-K
409 BTU-in/hr-ft²-°F
Melting Point 183 - 189 °C
361 - 372 °F
Solidus 183 °C
361 °F
Liquidus 189 °C
372 °F
Component Elements Properties Metric English Comments
Lead, Pb 20 %
20 %
Tin, Sn 80 %
80 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001246 ohm-cm
0.00001246 ohm-cm