Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GF30-60 42LH-NBK1 30% Glass Fiber Reinforced Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF30-60 42LH-NBK1 30% Glass Fiber Reinforced Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183-87
Filler Content 30 %
30 %
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.011 cm/cm
0.0070 - 0.011 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 225 MPa
32600 psi
ISO 178-93
Flexural Modulus 8.80 GPa
1280 ksi
ISO 178-93
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-93