Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.520 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
Nylene® PA6 Impact Modified 323 HS Nylon 6
Extrusion Grade; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Data provided by the manufacturer.
Flexural Modulus 0.520 GPa
75.4 ksi
1% Strain Value from rotomolded samples; ASTM D790
NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin
Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin..
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin  (discontinued **)
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design, low temperature impact excellent.Data provided by the manufacturer.
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
NOVA Chemicals Sclair® 2318 LLDPE Injection Molding Resin  (discontinued **)
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Applications: Thin walled container lids and closures.Data provided by the manufacturer.
Flexural Modulus 0.520 GPa
75.4 ksi
1% Strain Value from rotomolded samples; ASTM D790
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin
Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin..
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
NOVA Chemicals Sclair® 8306 UV8D, 8306G UV8D MDPE Rotational Molding Resin  (discontinued **)
Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer.
Flexural Modulus 0.520 - 1.30 GPa
75.4 - 189 ksi
Average value: 0.850 GPa Grade Count:5
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
UBE P7115U Electronic Grade Nylon Copolymer Powder
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
UBE 7115U Nylon 6/12 Copolymer
Description: UBESTA Nylon 12 CopolymerInformation provided by UBE.
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
Ashley Polymers Ashlene® 734LD Nylon 6
A plasticized, highly flexible Nylon 6 with high impact resistance.Data provided by the manufacturer
Flexural Modulus 0.520 - 13.8 GPa
75.4 - 2000 ksi
Average value: 2.82 GPa Grade Count:27
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Flexural Modulus 0.520 GPa
75.4 ksi
ISO 178
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Copyright © lookpolymers.com All Rights Reserved