Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 60 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen HP562T Fiber (Spunbond) Grade Polypropylene
Moplen HP562T is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562T is a homopolymer particularly suitable f..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene
Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in t..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Entec Hypel® PELLD60/.925 LLDPE  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Melt Flow 60 g/10 min

@Load 1.20 kg,
Temperature 300 °C
60 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Covestro Makrolon® CD 2005 Polycarbonate, Optical/Compact Disc Grade  (discontinued **)
Injection molding grade with exceptionally good flow, for optical storage media such as CD.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and..
Melt Flow <= 60 g/10 min

@Load 10.0 kg,
Temperature 380 °C
<= 60 g/10 min

@Load 22.0 lb,
Temperature 716 °F
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Melt Flow 60 g/10 min
60 g/10 min
ASTM D1238
Hyosung Topilene S905H PP
S905H Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Inno-Comp INNOPOL® CS 2-9514 10% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-9514 is a 10% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9514 is dev..
Melt Flow 60 - 100 g/10 min

@Load 2.16 kg,
Temperature 170 °C
60 - 100 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level...
Melt Flow 60 - 110 g/10 min

@Load 21.6 kg,
Temperature 170 °C
60 - 110 g/10 min

@Load 47.6 lb,
Temperature 338 °F
DDIN 53.735
Lubrizol Advanced Materials Pearlbond® DAP 750/2 Thermoplastic Polyurethane
The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pelle..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer
Forms: PelletsProcessing Methods:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 275 °C
60 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Melt Flow 60 - 100 g/10 min

@Load 2.16 kg,
Temperature 170 °C
60 - 100 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Lubrizol Advanced Materials PEARLBOND® 123 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 123 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit..
Melt Flow 60 - 100 g/10 min

@Load 2.16 kg,
Temperature 170 °C
60 - 100 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Lubrizol Advanced Materials PEARLBOND® 503 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 503 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli..
Melt Flow 60 g/10 min
60 g/10 min
ASTM D1238
SPS Guang Zhou POPTREEâ„¢ 6001 Flame-retarded Polyethylene
Characteristic: Low density, superior melt flow index, high notched impact strengthApplications: X'mas decorative productInformation Provided by SPS (Guang Zhou) Ltd.
Melt Flow 60 g/10 min

@Load 10.0 kg,
Temperature 250 °C
60 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® TN-1200 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 235 °C
60 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
Samyang Tribit® 1501N PBT, Flame Retardancy
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1501N is a V-2 flame retardancy grade.Appli..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Total Lumicene® MR60MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Lumicene® MR60MC2 is a metallocene random copolymer with a melt flow index of 60 g/10 min for injection molding. Lumicene® MR60MC2 differs from standard random copolymers by its molding reproducib..
Melt Flow 60 g/10 min

@Load 1.00 kg,
Temperature 190 °C
60 g/10 min

@Load 2.20 lb,
Temperature 374 °F
ASTM D1238R
UBE 7115U Nylon 6/12 Copolymer
Description: UBESTA Nylon 12 CopolymerInformation provided by UBE.
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 160 °C
60 g/10 min

@Load 4.76 lb,
Temperature 320 °F
cm<sup>3</sup>/10 min; ISO 1133
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melt Flow 60 g/10 min

@Load 2.16 kg
60 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Dow DOWLEX™ IP-60 High Density Polyethylene
DOWLEX® IP-60 resin is an improved processing high density polyethylene resin designed to offer excellent processability, good impact and top load strength required in thin wall injection molding. ..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Clariant Renol CPPR02096 Color concentrate of Titanium Oxide
Application to PolypropyleneData provided by Clariant Masterbatches
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 275 °C
60 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 275 °C
60 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced
15% Glass fiber reinforced and 25% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the followi..
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 275 °C
60 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 TF10 Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
Melt Flow 60 - 75 g/10 min
60 - 75 g/10 min
ISO 1133
Beijing Ranger Chem BLUESTAR® 1079 PBT
Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co.
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 275 °C
60 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 275 °C
60 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 MCS HI Polyamide 6 - Impact Modified
Very high impact resistance, cold impact grade (to -40°C). Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has t..
Melt Flow 60 g/10 min
60 g/10 min
ASTM D1238
Huntsman PE2072 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, gloss, and stiffness.Applications: Injection molding: lids and difficult to fill applications...
Melt Flow 60 - 100 g/10 min

@Load 2.16 kg,
Temperature 170 °C
60 - 100 g/10 min

@Load 4.76 lb,
Temperature 338 °F
DDIN 53.735
Lubrizol Advanced Materials Pearlbond® D183 Thermoplastic Polyurethane  (discontinued **)
The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo..
Copyright © lookpolymers.com All Rights Reserved