Polymer Property : Thermal Conductivity = 0.507 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® FTD-200 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® FTD-250 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SI-100 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SI-130 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SI-160 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SI-200 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SI-250 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SI-310 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SI-350 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SID-160Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SID-230Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SID-311Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SID-350Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® W-25 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® W-30 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® IGD-101 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Thermal Conductivity 0.0730 - 0.125 W/m-K
0.507 - 0.868 BTU-in/hr-ft²-°F
Trelleborg AEM Eccospheres® SID-120Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..