Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 62.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® FTD-200 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® FTD-250 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® FTD-250 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-100 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-100 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-130 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-160 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-160 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-200 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-200 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-250 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-250 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SI-350 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-160Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-160Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-230Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-230Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-311Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-311Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-350Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-350Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® W-25 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® W-30 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® W-30 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® IGD-101 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® IGD-101 Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-120Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..
Modulus of Elasticity 62.0 GPa
<br>@Temperature 25.0 °C
8990 ksi
<br>@Temperature 77.0 °F
Trelleborg AEM Eccospheres® SID-120Z Sodium Borosilicate Glass Microspheres
Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific..