Material Notes:
General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a wide range of both oxidizing and reducing environments. The high nickel content also provides resistance to chloride stress corrosion cracking.Molybdenum and copper are present in the alloy for increased resistance to pitting and crevice corrosion and to general corrosion in reducing acids.The low carbon content of 904L provides resistance to intergranular corrosion in the post-welded or stress relieved condition.ApplicationsThe corrosion resistance of 904L makes it a useful alloy in numerous severe operating environments. It is utilized extensively in the chemical, petrochemical, pulp and paper, and pollution control industries :Tanks, vessels, piping, heat exchangers, and other equipment for the production and handling of sulfuric and phosphoric acid.Reactor vessels for fertilizer productionTall oil distillationPulp and paper bleaching operationsAbsorber towers, stack linings, duct work, dampers, and other support equipment for flue gas desulphurization systems for fossil-fired power plants and waste incinerators.Information provided by Carlson
Physical Properties Metric English Comments
Density 7.97 g/cc
0.288 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 192
<= 192
Hardness, Rockwell B <= 90
<= 90
Tensile Strength at Break >= 490 MPa
>= 71000 psi
Tensile Strength, Yield >= 214 MPa

@Strain 0.200 %
>= 31000 psi

@Strain 0.200 %
Elongation at Break >= 35 %
>= 35 %
Reduction of Area >= 40 %
>= 40 %
Modulus of Elasticity 196 GPa
28400 ksi
Thermal Properties Metric English Comments
CTE, linear 10.4 µm/m-°C

@Temperature 20.0 - 98.9 °C
5.80 µin/in-°F

@Temperature 68.0 - 210 °F
14.6 µm/m-°C

@Temperature 20.0 - 399 °C
8.10 µin/in-°F

@Temperature 68.0 - 750 °F
16.6 µm/m-°C

@Temperature 20.0 - 799 °C
9.20 µin/in-°F

@Temperature 68.0 - 1470 °F
Specific Heat Capacity 0.439 J/g-°C

@Temperature 20.0 °C
0.105 BTU/lb-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.020 %
<= 0.020 %
Chromium, Cr 19 - 23 %
19 - 23 %
Copper, Cu 1.0 - 2.0 %
1.0 - 2.0 %
Iron, Fe 38.9 - 53 %
38.9 - 53 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo 4.0 - 5.0 %
4.0 - 5.0 %
Nickel, Ni 23 - 28 %
23 - 28 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.035 %
<= 0.035 %