Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives Turbo Fuse Series 110SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO FUSE SERIES
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives Turbo Fuse Series 110SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications. The fast curing qualities make it especially desirable in high speed industrial production. Turbo Fuse is ideal for use in applications that require good "wicking" characteristics and/or in close fitting applications. Because of TurboFuse 110SI Series low viscosity, it works especially well in close fitting applications such as metal to metal bonding, and rubber to rubber such as "O" ring repair/manufacture.Part Numbers for this data: 04-110SI, 10-110SI, 15-110SI, 20-110SI, 25-110SI, 30-110SI, 35-110SISoluble in Acetone, MEK, Amide, Methylene ChlorideInformation provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid State
Viscosity 2.0 - 5.0 cP
2.0 - 5.0 cP
Liquid State
Mechanical Properties Metric English Comments
Hardness, Barcol 65
65
Cured State
Shear Strength 17.2 MPa
2500 psi
Tensile, (Cured State)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Cured State
Softening Point 149 °C
300 °F
Cured State
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cured State
Flash Point 76.7 - 93.3 °C
170 - 200 °F
Liquid State (Tagliabue closed cup)
Electrical Properties Metric English Comments
Dielectric Constant 3.33

@Frequency 1.00e+6 Hz
3.33

@Frequency 1.00e+6 Hz
Cured State
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Liquid State
Descriptive Properties Value Comments
Appearance Clear liquid
Liquid State
Clear-Hard
Cured State
Base compound (Resin) Surface Insensitive Ethyl Cyanoacrylate
Liquid State
Gap Fill 0.002"
Cured State
Material Set Up Time <3 sec
Rubber to Rubber
3-10 sec
Polycarbonate to Polycarbonate
3-5 sec
Phenolic to Phenolic
3-5 sec
Aluminum to Aluminum
5-15 sec
Steel to Steel