Material Notes:
ATOFINA Polypropylene PPH 5060 is homopolymer.ApplicationATOFINA Polypropylene PPH 5060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 5060 is also a general purpose injection grade for molding technical items.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ISO 2039-2
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.50 GPa
218 ksi
ISO 527-2
Flexural Modulus 1.40 GPa
203 ksi
ISO 527-2
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 164 °C
327 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
120°C per hour; ISO 75-2
Vicat Softening Point 85.0 °C
185 °F
50N-50°C per hour; ISO 306
150 °C
302 °F
10N-50°C per hour; ISO 306