Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPC
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids combining flexibility and low warpage.Polypropylene PPC 8780 is also suitable for extrusion coating.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 18 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
18 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ISO 2039-2
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Elongation at Yield 5.5 %
5.5 %
ISO 527-2
Tensile Modulus 1.05 GPa
152 ksi
ISO 527-2
Flexural Modulus 0.950 GPa
138 ksi
ISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²
<br>@Temperature -20.0 °C
2.62 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 180
11.0 kJ/m²
<br>@Temperature 23.0 °C
5.23 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature 23.0 °C
6.66 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
1.60 J/cm²
<br>@Temperature -20.0 °C
7.61 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
120°C per hour; ISO 752
Vicat Softening Point 65.0 °C
<br>@Load 5.10 kg
149 °F
<br>@Load 11.2 lb
50°C per hour; ISO 306
135 °C
<br>@Load 1.02 kg
275 °F
<br>@Load 2.25 lb
50°C per hour; ISO 306