Panipol Oy DXH-PP Inherently Conductive Polymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Panipol
Trade Name Oy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Panipol Oy DXH-PP Inherently Conductive Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are controllable resistance in optimal ESD protection range 10^6-10^9 O, low sloughing and limited colorablity. the conductivity of Panipol DXH-PP / matrix polymer blend is tunable from insulators into matrix polymer chain instead of acting as a filler. The conductive/dissipative property is permanent and built into the polymer chain. Panipol DXH-PP has been developed mainly for injection molding applications. Panipol DXH-PP should be used in 10-18% ratio with PP Heterophasic copolymer to achieve surface resistance values from 10^6 to 10^10 O, (IEC 61340-5-1d). The products made out of Panipol DXH-PP are resusable and recyclable. Typical applications include injection moulded boxes and bins etc. giving permanent ESD protection for the various packaging applications.Information provided by Panipol Oy Ltd
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 180
Electrical Properties Metric English Comments
Surface Resistance 1.00e+6 - 1.00e+7 ohm

@Thickness 2.00 mm
1.00e+6 - 1.00e+7 ohm

@Thickness 0.0787 in
sheet; IEC 61340-5-1
Static Decay <= 0.50 sec

@Thickness 2.00 mm
<= 0.50 sec

@Thickness 0.0787 in
sheet; IEC 61340-5-1
Processing Properties Metric English Comments
Front Barrel Temperature 190 - 220 °C
374 - 428 °F
Melt Temperature <= 230 °C
<= 446 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Descriptive Properties Value Comments
Back Pressure High
Injection Speed High
Plasticizing Speed High