Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C); Injection Rate: Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Melt Flow 5.00 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.00 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Tensile Stress 4.83 MPa

@Strain 300 %
700 psi

@Strain 300 %
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 232 °C
360 - 450 °F
Middle Barrel Temperature 188 - 238 °C
370 - 460 °F
Front Barrel Temperature 193 - 243 °C
380 - 470 °F
Nozzle Temperature 199 - 249 °C
390 - 480 °F
Zone 1 182 - 232 °C
360 - 450 °F
Zone 2 188 - 238 °C
370 - 460 °F
Zone 3 193 - 243 °C
380 - 470 °F
Zone 5 199 - 249 °C
390 - 480 °F
Die Temperature 199 - 249 °C
390 - 480 °F
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Injection Pressure 1.38 - 5.52 MPa
200 - 800 psi
Back Pressure 0.172 - 0.689 MPa
25.0 - 100 psi
Cushion 0.381 - 2.54 cm
0.150 - 1.00 in
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments
Appearance Translucent