Material Notes:
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: Temperature Rating: 60°CInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 seconds; ASTM D2240
Tensile Strength at Break 15.0 MPa
2170 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous Use; ASTM D794
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
UL RTI, Electrical 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
UL RTI, Mechanical with Impact 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
UL RTI, Mechanical without Impact 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 24 %
24 %
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Clear/Transparent