Material Notes:
Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 127
127
ASTM D785
Tensile Strength, Yield 117 MPa
17000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 162 MPa
23500 psi
ASTM D790
Flexural Modulus 5.31 GPa
770 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
30.0 µin/in-°F
ASTM D696
Melting Point 310 °C
590 °F
Maximum Service Temperature, Inert 160 °C
320 °F
ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 277 °C
531 °F
Unannealed; ASTM D648