| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
PolyOne LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5.1 mm/min; ASTM D638 |
|
PolyOne Nymax™ GMF 600 40 Black 117 V P1 Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 MF25 Glass/Mineral Filled Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release
Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Tensile Strength, Yield |
117
MPa @Temperature 23.0 °C |
17000
psi @Temperature 73.4 °F |
ISO 527 |
|
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**)
Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
|
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu
Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding
Information provided by PolyOne™ Corporation
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
(disco
Information provided by PolyOne™ Corporation
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | 2.0 in/min; ASTM D638 |
|
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled
30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON DE0026E PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE0026E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ISO 527 |
|
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
Techmer ES HiFill® ABS GF60 LE 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | 5 mm/min; ISO 527 |
|
SABIC Innovative Plastics Valox® SHF436HR PBT
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East)
PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
Techmer ES Plastiblend® TPX-HTN-000CB 15% Glass Filled
Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
SABIC Innovative Plastics LNP VERTON MX02795 PP (Asia Pacific)
LNP* Verton* MX02795 is a compound based on Polypropylene resin containing Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics NORYL GTX870 PPE+PA6 (Asia Pacific) |
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D 638 |
|
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ISO 527 |
|
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | SABIC - Japan Method |
|
SABIC Innovative Plastics NORYL GFN3L PPE+HIPS (Asia Pacific)
PPE+PS, GF30%, hydrolytic stability improved
|
|||
| Tensile Strength, Yield | 117 - 221 MPa | 17000 - 32000 psi | 0.2% offset |
|
Eagle Brass 19210 XP-10 Copper Iron, Annealed
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
|
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
|
|||
| Tensile Strength, Yield |
117
MPa @Temperature -40.0 °C |
17000
psi @Temperature -40.0 °F |
ISO Data |
|
BASF Ultramid® 8253 HS PA6 (Dry)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..
|
|||
| Tensile Strength, Yield | 117 MPa | 17000 psi | ISO 527-2 |
|
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
|
|||