Material Notes:
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. The key features of Styrodur C are high compressive strength, low water absorption, and outstanding thermal insulation. It is also rot-proof and easy to handle on site. Compressive strength is the major factor that differentiates the various grades of Styrodur C.Applications: Cavity walls, Pitched roofs, Ceilings, and WarehouseInformation provided by BASF
Physical Properties Metric English Comments
Density 0.0300 g/cc
0.00108 lb/in³
Water Absorption 0.20 %
0.20 %
by immersion; DIN EN 12087
<= 3.0 %
<= 3.0 %
by diffusion; DIN EN 12088
Water Vapor Transmission 100 - 150 g/m²/day
6.44 - 9.66 g/100 in²/day
DIN EN 12086
Deformation <= 5.0 %
<br>@Pressure 0.0400 MPa,<br> Temperature 70.0 °C
<= 5.0 %
<br>@Pressure 5.80 psi,<br> Temperature 158 °F
DIN EN 1605
Mechanical Properties Metric English Comments
Creep Strength 0.100 MPa
<br>@Strain <=2.00 %
14.5 psi
<br>@Strain <=2.00 %
Compressive; DIN EN 1606
Compressive Strength 0.250 MPa
<br>@Strain 10.0 %
36.3 psi
<br>@Strain 10.0 %
DIN EN 826
Compressive Modulus 0.0150 GPa
2.18 ksi
Elasticity; Short term E; DIN EN 826
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 8.00 µm/m-°C
4.44 µin/in-°F
DIN 53752
CTE, linear, Transverse to Flow 6.00 µm/m-°C
3.33 µin/in-°F
DIN 53752
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
Moisture Content: 0%
0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 1%
0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 2%
0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 3%
0.0350 W/m-K
0.243 BTU-in/hr-ft²-°F
Moisture Content: 4%
0.0360 W/m-K
0.250 BTU-in/hr-ft²-°F
Moisture Content: 5%
0.0370 W/m-K
0.257 BTU-in/hr-ft²-°F
Moisture Content: 6%
0.0380 W/m-K
0.264 BTU-in/hr-ft²-°F
Moisture Content: 8%
0.0390 W/m-K
0.271 BTU-in/hr-ft²-°F
Moisture Content: 10%
0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
Moisture Content: 12%
0.0240 W/m-K
<br>@Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F
<br>@Temperature -112 °F
0.0260 W/m-K
<br>@Temperature -60.0 °C
0.180 BTU-in/hr-ft²-°F
<br>@Temperature -76.0 °F
0.0280 W/m-K
<br>@Temperature -40.0 °C
0.194 BTU-in/hr-ft²-°F
<br>@Temperature -40.0 °F
0.0300 W/m-K
<br>@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F
<br>@Temperature -4.00 °F
0.0320 W/m-K
<br>@Temperature 0.000 °C
0.222 BTU-in/hr-ft²-°F
<br>@Temperature 32.0 °F
0.0330 W/m-K
<br>@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F
<br>@Temperature 50.0 °F
0.0340 W/m-K
<br>@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F
<br>@Temperature 68.0 °F
0.0350 W/m-K
<br>@Temperature 30.0 °C
0.243 BTU-in/hr-ft²-°F
<br>@Temperature 86.0 °F
0.0360 W/m-K
<br>@Temperature 40.0 °C
0.250 BTU-in/hr-ft²-°F
<br>@Temperature 104 °F
0.0370 W/m-K
<br>@Temperature 50.0 °C
0.257 BTU-in/hr-ft²-°F
<br>@Temperature 122 °F
0.0310 W/m-K
<br>@Thickness 30.0 mm
0.215 BTU-in/hr-ft²-°F
<br>@Thickness 1.18 in
DIN EN 13164
0.0320 W/m-K
<br>@Thickness 40.0 mm
0.222 BTU-in/hr-ft²-°F
<br>@Thickness 1.57 in
DIN EN 13164
0.0330 W/m-K
<br>@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F
<br>@Thickness 1.97 in
DIN EN 13164
0.0340 W/m-K
<br>@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F
<br>@Thickness 2.36 in
DIN EN 13164
0.0350 W/m-K
<br>@Thickness 80.0 mm
0.243 BTU-in/hr-ft²-°F
<br>@Thickness 3.15 in
DIN EN 13164
Maximum Service Temperature, Air 75.0 °C
167 °F
DIN EN 14706
Descriptive Properties Value Comments
Commercial Status Europe
Dimensional Stability at Heat < 5%
70°C, 90% rh; DIN EN 1604
Freeze-Thaw-Resistance <1%
DIN EN1209