| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790 |
| Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790 |
| Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790 |
| Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790 |
| Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
| Flexural Strength | 64.1 MPa @Thickness 3.17 mm |
9300 psi @Thickness 0.125 in |
ASTM D790 |
| PTS Trilac® FR1 ABS- Flame Retardant ABS Resin
(Unverified Data**) Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790 |
| Techmer ES Plaslube® AC-80/TF/10 NAT Acetal (POM) Copolymer |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790 |
| Techmer ES Plaslube® AC-80/TF/20 BK1941 Acetal (POM) Copolymer |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790 |
| Techmer ES Plaslube® AC-80/TF/20 NAT Acetal (POM) Copolymer |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | Method I (3 point load), 1.3 mm/min; ASTM D790 |
| Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D638 |
| Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
| Flexural Strength | 64.1 MPa | 9300 psi | ASTM D790B |
| Chevron Phillips EA3400 Medium Flow Crystal DescriptionChevron EA3400 is a medium flow-crystal polystyrene resin developed to blend with Styrene-Butadiene block copolymers for sheet extrusion and vacuum thermoforming. EA3400 can be used in c.. |
|||