Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ASTM D792
Water Absorption 0.17 %

@Time 86400 sec
0.17 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 230 MPa
33400 psi
ASTM D638
Elongation at Yield 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 331 MPa
48000 psi
ASTM D790
Flexural Modulus 13.4 GPa
1950 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.2 µm/m-°C
19.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 288 °C
550 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+15 ohm-cm
8.00e+15 ohm-cm
ASTM D257
Dielectric Strength 21.7 kV/mm
550 kV/in
Method A (Short-Time); ASTM D149