Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.020 cm/cm

@Thickness 3.17 mm
0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Yield Strength 33.8 MPa
4900 psi
ASTM D790
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 66.6 µm/m-°C
37.0 µin/in-°F
ASTM D696
Melting Point 170 °C
338 °F
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149