Eagle Brass 425 Tin Brass 2%, Extra Spring

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Eagle Brass 425 Tin Brass 2%, Extra Spring.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connectors and terminals.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.77 g/cc
0.317 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T >= 76
>= 76
Thickness > 0.020 Inch
Tensile Strength, Ultimate >= 634 MPa
>= 92000 psi
Tensile Strength, Yield >= 600 MPa
>= 87000 psi
0.2% offset
Elongation at Break >= 1.0 %
>= 1.0 %
in 2 in.
Tensile Modulus 110 GPa
16000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 119 W/m-K
828 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 88.5 %
88.5 %
Tin, Sn 2.0 %
2.0 %
Zinc, Zn 9.5 %
9.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed