| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 103 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific)
Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific)
Nonhalogenated. 17.5 MFR, for small intricate parts.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 131 PC (Asia Pacific)
Nonhalogenated. 3.5 MFR.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 134R PC
Nonhalogenated. 3.5 MFR. Internal mold release. FDA food contact compliant in limited colors.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 153 PC (Asia Pacific)
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific)
7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 221 PC (Asia Pacific)
17.5 MFR, for small, intricate parts. Improved flame retardance.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 223R PC
17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 241R PC
General purpose polycarbonate with 10.5 MFR and internal mold release.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 945AU PC (Asia Pacific)
Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® FXE154 PC
FDA compliant (color limited) PC. 2.5 MFR. Potable water/extrusion blowmoldable. ILLUMINATE special effects (fluorescent/edge glow colors).
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East)
Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope..
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML5221 PC
General Purpose High Flow Polycarbonate Powder Grade.This data was supplied by SABIC-IP for the Americas region.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML6076 PC
Passes FAR 25.853: 60 seconds at 30 mil.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 925A PC (Asia Pacific)
Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran..
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific)
Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit..
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific)
Opaque colors, high viscosity, superior flame retardance. UV-stabilized.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 953A PC (Asia Pacific)
Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® ML4248 PC
Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Extrusion grade. Transparent, transluscent and opaque colors.
|
|||
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
|
Techmer ES Electrablend® PA6/6 CF20 L BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf..
|
|||
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
|
Techmer ES HiFill FR® PC FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection Molding Appearance: Clear/TransparentInformation provided by TP Composites, Inc.
|
|||
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
|
Techmer ES HiFill FR® PC FR X
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Flame Retardant and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
|
Techmer ES Plastiblend® TPX-HTN-000CA
Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature 20.0 °C
|
38.0
µin/in-°F <br>@Temperature 68.0 °F
|
ASTM data |
|
Styron CALIBREâ„¢ 200 10 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature 20.0 °C
|
38.0
µin/in-°F <br>@Temperature 68.0 °F
|
ASTM data |
|
Styron CALIBREâ„¢ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant
CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g..
|
|||
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
|
Techmer ES Elastoblend® PC IM
Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified Processing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
|
Techmer ES HiFill FR® PC FR UG X GY158
Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame Retardant and Good Mold ReleaseAppearance: GreyInformation provided by TP Composites, Inc.
|
|||
| CTE, linear, Parallel to Flow |
68.4
µm/m-°C <br>@Temperature -40.0 - 95.0 °C
|
38.0
µin/in-°F <br>@Temperature -40.0 - 203 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics Lexan® 243R PC
10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release.
|
|||