| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D 648 |
|
NOVA Chemicals Surpass® RMs341-U Octene sHDPE Rotational Molding Resin
RMs341-U complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341-..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ISO 75-1/-2 |
|
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**)
Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
|
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade
(discontinued **)
ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 - 82.0 °C | 144 - 180 °F | Average value: 74.6 °C Grade Count:12 |
|
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
LyondellBasell Alathon® L5332CP High Density Polyethylene
ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resis..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade
ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applic..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648-97 |
|
Ipiranga Petrochem MB 0310 MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
LyondellBasell Hifaxâ„¢ ETA-3131EUV Thermoplastic Olefin Resin
Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processability, exc..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ISO 75 |
|
Styrolution Styrolux 3G55 SBC
Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
62.0
°C <br>@Thickness 3.20 mm
|
144
°F <br>@Thickness 0.126 in
|
ISO 75 |
|
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
62.0
°C <br>@Thickness 3.20 mm
|
144
°F <br>@Thickness 0.126 in
|
ISO 75 |
|
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
62.0
°C <br>@Thickness 3.20 mm
|
144
°F <br>@Thickness 0.126 in
|
ISO 75 |
|
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
62.0
°C <br>@Thickness 3.20 mm
|
144
°F <br>@Thickness 0.126 in
|
ISO 75 |
|
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
62.0
°C <br>@Thickness 3.20 mm
|
144
°F <br>@Thickness 0.126 in
|
ISO 75 |
|
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | dry; ISO 75-1/-2 |
|
DSM Novamid® ST145 NAT PA6-I
Impact Modified, Injection Molding
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
ExxonMobil LL 8460.29 Rotational Molding Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
|
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
|
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
ExxonMobil LLP8460.29 Rotational Molding Resin
Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | 0.125";; ASTM D648 |
|
Diamond Polymers NPP11-0242 Polyethylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
|
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE)
Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
3D Systems Accura® Xtreme Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
|
Aclo Accucomp Polyethylene HD0200L High Density |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.2 °C | 144 °F | ASTM D648 |
|
Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | |
|
BASF Novolen® 2900 H Polypropylene
Injection molded and thermoformed parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
62.0
°C <br>@Thickness 4.00 mm
|
144
°F <br>@Thickness 0.157 in
|
after annealing 150°C 16 hr; ASTM D648 |
|
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **)
Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **)
LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ASTM D648 |
|
Formosa Plastics Formolene® L64220U Rotational Molding LLDPE
(discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L64220U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase ProcessTM. Th..
|
|||