| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 72.0 °C @Load 1.00 kg |
162 °F @Load 2.20 lb |
ISO 306/A |
| Polimeri Europa Greenflex® ML 31 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion Greenflex ML 31 is an ethylene vinyl acetate copolymer (EVA) for injection molding applications and extrusion profile. Greenflex ML 31 contains additive waxes to obtain high production speed.Main A.. |
|||
| Vicat Softening Point | 72.0 °C @Load 1.00 kg |
162 °F @Load 2.20 lb |
ISO 306/A |
| Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
| DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
| Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
| Karina E818-10/23-CRM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
| Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
| Karina E818-18/99-CRM Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | |
| LyondellBasell Lupolen® 4152 D SW 00413 HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
| Mitsui ADMER® AT1053A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
| Mitsui ADMER® NF528A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
| Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
| Karina 806-48/1-BY-ERYB Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
| Vicat Softening Point | >= 72.0 °C | >= 162 °F | ASTM D 1525 |
| Karina E 818-10/23-CRM-AS White PVC Compound UV. protection addedInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ISO 306 |
| Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene I3 (HC 7260) is a high density polyethylene with propylene as comonomer. The product has good impact strength, good stress cracking resistance, low warping and good flow ability as well as high dens.. |
|||
| Vicat Softening Point | 72.2 °C | 162 °F | ASTM D1525 |
| Teknor Apex Sinvicomp SBF 3779 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |
|||
| Vicat Softening Point | 72.0 °C @Load 5.10 kg |
162 °F @Load 11.2 lb |
B50; ISO 306 |
| Borealis Borstar® HE3410 HDPE for Sewage Pipes Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | B (50N); ISO 306 |
| Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ISO 306 |
| Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T.. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ISO 306 |
| Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
| DuPont Appeel® LSR11D554 Lidding Sealant Resin Appeel® LSR11D554 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals to poly.. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | A50; DIN 53460 |
| Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |
|||
| Vicat Softening Point | 72.2 °C | 162 °F | ASTM D1525 |
| ExxonMobil Escorene™ FL 00212 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00212 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 260°C (500°F) may cause resin degradation. Machines should always b.. |
|||
| Vicat Softening Point | 72.2 °C | 162 °F | ASTM D1525 |
| ExxonMobil Escorene™ FL 00909 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00909 is used in extrusion coating, cast film and co-extrusion. FL 00909 is good sealing material with good optical properties.Processing Conditions: Excellent results are ob.. |
|||
| Vicat Softening Point | 72.2 °C | 162 °F | ISO 306 |
| ExxonMobil LDPE LD 655 Low Density Polyethylene Resin (European Grade) Product Description: LD 655 is a very high flow LDPE grade with a very good flexibility. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabiliz.. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | JIS-K-6740 |
| Denka VINYKON M4000 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
| Vicat Softening Point | 72.2 °C | 162 °F | |
| Dow Primacor® 3460 Ethylene Acrylic Acid (EAA) PRIMACOR® 3460 polymer containing 9.5% comonomer is a heat seal coating for high speed packaging applications where low temperature processing is necessary for minimal taste and odor effects. It is.. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | |
| BASF Novolen® 3200 MC Polypropylene Cast film without slip and blocking agents.Data was collected by ISO methods and provided by BASF. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | |
| BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
| Vicat Softening Point | 72.2 °C | 162 °F | ASTM D1525 |
| Teknor Apex Sinvicomp SBF 3778 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | |
| BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | A50; DIN 53460 |
| Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | A50; DIN 53460 |
| Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
| Vicat Softening Point | 72.0 °C | 162 °F | ASTM D1525 |
| DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||