Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of this alloy.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.44 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 951 MPa
138000 psi
Tensile Strength, Yield 563 MPa

@Strain 0.200 %
81700 psi

@Strain 0.200 %
Elongation at Break 46 %
46 %
Modulus of Elasticity 208 GPa
30200 ksi
Poissons Ratio 0.28
0.28
Shear Modulus 81.4 GPa
11800 ksi
Thermal Properties Metric English Comments
CTE, linear 12.8 µm/m-°C

@Temperature 21.0 - 100 °C
7.11 µin/in-°F

@Temperature 69.8 - 212 °F
Mean
13.3 µm/m-°C

@Temperature 21.0 - 300 °C
7.39 µin/in-°F

@Temperature 69.8 - 572 °F
Mean
13.9 µm/m-°C

@Temperature 21.0 - 500 °C
7.72 µin/in-°F

@Temperature 69.8 - 932 °F
Mean
14.9 µm/m-°C

@Temperature 21.0 - 700 °C
8.28 µin/in-°F

@Temperature 69.8 - 1290 °F
Mean
Specific Heat Capacity 0.410 J/g-°C
0.0980 BTU/lb-°F
Thermal Conductivity 9.70 W/m-K
67.3 BTU-in/hr-ft²-°F
Melting Point 1290 - 1350 °C
2350 - 2460 °F
Solidus 1290 °C
2350 °F
Liquidus 1350 °C
2460 °F
Maximum Service Temperature, Air 650 °C
1200 °F
resistance to low cycle and thermal fatigue
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.40 %
<= 0.40 %
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 20 - 23 %
20 - 23 %
Cobalt, Co <= 1.0 %
<= 1.0 %
Iron, Fe <= 5.0 %
<= 5.0 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Molybdenum, Mo 8.0 - 10 %
8.0 - 10 %
Nickel, Ni >= 58 %
>= 58 %
Niobium, Nb (Columbium, Cb) 3.15 - 4.15 %
3.15 - 4.15 %
Includes Ta
Nitrogen, N <= 0.020 %
<= 0.020 %
Phosphorous, P <= 0.015 %
<= 0.015 %
Silicon, Si <= 0.020 %
<= 0.020 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti <= 0.40 %
<= 0.40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000132 ohm-cm
0.000132 ohm-cm
Magnetic Permeability 1.0006
1.0006
at 200 Oersted (15.9 kA/m)