Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurofoam Porocell POR 304 B EPDM Foam

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eurofoam s.r.l.
Trade Name POROCELL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Porocell POR 304 B EPDM Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.110 - 0.150 g/cc
0.00397 - 0.00542 lb/in³
ISO 845-88
Water Absorption <= 3.0 %
<= 3.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 50 - 60
50 - 60
ASTM D 2240
Tensile Strength 0.600 MPa
87.0 psi
ASTM D 412
Elongation at Break >= 120 %
>= 120 %
ASTM D 412
Compressive Yield Strength 0.0420 MPa

@Strain 25.0 %
6.09 psi

@Strain 25.0 %
ASTM 1056/85
Tear Strength 0.450 kN/m
2.57 pli
ASTM D 624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
ASTM D 3575
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
ASTM D 3575
Shrinkage <= 4.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 4.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Fire Resistance MV22 302
Pass
Vulcanization Sulfur
Users viewing this material also viewed the following: