Bisalloy Steels BisPlate 70 Thickness >80-100 mm

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel , Carbon Steel , Low Carbon Steel
Manufacturer Bisalloy Steels
Trade Name BisPlate
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bisalloy Steels BisPlate 70 Thickness >80-100 mm.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperature fracture toughness.Applications: Transport Equipment, Storage Tanks, High Rise Buildings, Lifting Equipment, Mining Equipment, Longwall Mining SupportsTesting: AS/NZS 3597 Grade 600 NATA approvedWelding: According to AS/NZS 1554 parts 4 and 5Tolerance: In accordance with AS/NZS 1365
Mechanical Properties Metric English Comments
Hardness, Brinell 230
230
Tensile Strength at Break 760 MPa
110000 psi
Tensile Strength, Yield 670 MPa

@Strain 0.200 %
97200 psi

@Strain 0.200 %
Elongation at Break 28 %
28 %
in 50 mm GL
Charpy Impact 180 J

@Temperature -20.0 °C
133 ft-lb

@Temperature -4.00 °F
Longitudinal
Component Elements Properties Metric English Comments
Boron, B 0.0010 %
0.0010 %
Carbon, C 0.16 %
0.16 %
Chromium, Cr 0.90 %
0.90 %
Iron, Fe 97.4 %
97.4 %
As Balance
Manganese, Mn 1.15 %
1.15 %
Molybdenum, Mo 0.20 %
0.20 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0030 %
0.0030 %
Descriptive Properties Value Comments
CE (IIW) 0.58
PCM 0.3
Surface Finish Shotblasted