Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Omni Plastics OmniTuff™ CPP TF30 Copolymer Polypropylene Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Omni Plastics
Trade Name OmniTuff™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniTuff™ CPP TF30 Copolymer Polypropylene Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.3 MPa
4250 psi
ASTM D638
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256