Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 12.4 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.4 GPa
1800 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® PC-15CF-15GF/000 Polycarbonate (PC)
Information provided by PolyOne
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant  (discontinued **)
Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr..
Tensile Modulus 12.4 GPa
1800 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
Tensile Modulus 12.4 GPa
1800 ksi
5 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Plenco 1500 Polyester, Granular, Compression Molded
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon..
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Tensile Modulus 12.4 GPa
1800 ksi
1 mm/min
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Dry)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Applied Composites 8041 Polyester SMC
Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: UL 94-VO, Radiant Panel
Tensile Modulus 12.4 GPa
1800 ksi
1 mm/min
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
Tensile Modulus 12.4 GPa

@Treatment Temp. 70.0 °C,
Time 180000 sec
1800 ksi

@Treatment Temp. 158 °F,
Time 50.0 hour
62% rel. humidity
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Tensile Modulus 12.4 GPa
1800 ksi
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..