| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
IDI Composites 46-12 Thermoset Polyester, Molding
Highest strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer.
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r..
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Plenco 3303 Phenolic, Granular, Compression Molded
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b..
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Plenco 3356 Phenolic, Granular, Injection Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Plenco 3356 Phenolic, Granular, Transfer Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret..
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Resinoid 2016P Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
|
|||
| Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
|
Resinoid 2020 Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
|
|||
| Compressive Strength | 159 MPa | 23100 psi | Conditioned; ASTM D695 |
|
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..
|
|||