Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Polymax® Maxelast® P3653T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Polymax® Maxelast® P3855 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield >= 8.27 MPa
>= 1200 psi
ASTM D638
S&E Specialty Polymers GTPO8290-GT7 PVC
Application: 80°C, Low Smoke, Zero Halogen, Flame Retardant Polyethylene Compound for extrusion applications.    Specifically designed to withstand severe UV exposure while maintaining very good ..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Polymax® Maxelast® P3975H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Polymax® Maxelast® C4880 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Strength, Yield 8.27 MPa
1200 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 661 Perfluoroelastomer
Chemraz® 661 perfluoroelastomer is specifically developed by Greene Tweed to meet the unique demands of aggressive plasma systems. This product’s unique formulation provides enhanced plasma..
Tensile Strength, Yield 8.27 MPa
1200 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7455 ER TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tensile Strength, Yield 8.27 MPa
1200 psi
Spartech E65050 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Tensile Strength, Yield 8.27 MPa
1200 psi
Tensile strength decreases by 25% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9275 High Performance Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex APEX® 3201-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 8.27 MPa
1200 psi
100%; ASTM D412
Teknor Apex APEX® 3201-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex APEX® 3210-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex APEX® 3301-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 8.27 MPa
1200 psi
100%; ASTM D412
Teknor Apex APEX® 3302-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
Tensile Strength, Yield 8.27 MPa
1200 psi
100%; ASTM D412
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Tensile Strength, Yield 8.27 MPa
1200 psi
100%; ASTM D412
Teknor Apex MF 165 D NT Polyvinyl Chloride, Flexible Film
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex MONPRENE® MP 2840M Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield >= 8.27 MPa
>= 1200 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7157 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 8.27 MPa
1200 psi
Tensile strength decreases by 20% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412-92
Saint-Gobain Versilicâ„¢ SPX-70I.B. High Strength Silicone Pressure Tubing Formulation
Description: Versilicâ„¢ SPX-70 I.B.: Produced form a proprietary combination of silicone elastomers, Versilicâ„¢ SPX-70 I.B. Tubing optimizes critical physical properties such as tensile st..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex TEKBOND® 6000-60 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex TEKBOND® MP 1728 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex TEKBOND® MP 1728 UVF Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex UNIPRENE® 7100-80 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
Tensile Strength, Yield 8.27 MPa

@Temperature 21.1 °C
1200 psi

@Temperature 70.0 °F
Flatwise Tensile
Hexcel® Redux® 308A-NA Modified epoxy film adhesive
Redux 308A-NA is a high-strength, flow-controlled film adhesive with flexible cure schedules at 300°F or 350°F. Redux 308A-NA contains glass beads that give good flow control. It is suitable for m..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412
Teknor Apex UNIPRENE® 7010-80 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 8.27 MPa
1200 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow 722 Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c..
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D-638
Axiall 8554 Moldings & Extrusions Flexible PVC
General purpose, jelly clear flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 8.27 MPa
1200 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT 38-074 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:Hot Runner MoldingFDA (Food Contact)Teething ring & pacifierMulti-PurposeMarket:Consumer GoodsProcessing Method:I..
Copyright © lookpolymers.com All Rights Reserved