Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning HS III BASE & 10:1 CLEAR CATALYST

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning HS III BASE & 10:1 CLEAR CATALYST.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High strength lower durometer silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items. HS III Base with HS III 10:1 Clear Catalyst is recommended for use with polyesters and plaster or wax.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc

@Temperature 25.0 °C
1.16 g/cc

@Temperature 77.0 °F
Viscosity 16000 cP
16000 cP
dynamic, mixing
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
Tensile Strength, Ultimate 2.41 MPa
350 psi
Elongation at Break 550 %
550 %
Tear Strength 17.5 kN/m
100 pli
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Working Time (min) 120
Users viewing this material also viewed the following: