Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QGel 310 QSI Quantum Silicones High Strength Gel

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ACC QGel 310 QSI Quantum Silicones High Strength Gel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection. Key Features: 24 hour room temperature or heat cure One to one mix ratio Soft but resilient Dispensing equipment not necessaryPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
"B" component
0.970 g/cc
0.970 g/cc
"A" component
Viscosity 1000 cP
1000 cP
"B" component
1000 cP
1000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Penetration 5.0 - 9.0
5.0 - 9.0
mm, 30 mins @ 150°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 19.2 kV/mm
487 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
60.0 min

@Temperature 100 °C
1.00 hour

@Temperature 212 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Gel Time 45.0 min
45.0 min
Descriptive Properties Value Comments
Color Transparent
"A" component
Transparent
"B" component