Material Notes:
Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.Specific Characteristics: Flammability according to CSN EN ISO 11925-2, class E and DIN 4102-B1. Shorter processing cycle than for type 1020F.Typica Application: Large-size molded blocks. Molded boards. Cut boards and building insulation profiles acc CSN EN 13163Synthos was formerly known as Kaucuk. All information provided by Synthos.
Physical Properties Metric English Comments
Bulk Density 0.0160 g/cc
0.000578 lb/in³
Minimum
0.0160 - 0.0400 g/cc
0.000578 - 0.00145 lb/in³
Typical
Particle Size 900 - 1250 µm
900 - 1250 µm