Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPS Guang Zhou PONYLâ„¢ EP4003G10 Non-halogen flame retardance/GF10%-PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer SPS Guang Zhou
Trade Name PONYL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou PONYLâ„¢ EP4003G10 Non-halogen flame retardance/GF10%-PA66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristic: Good flame retardance, high mechanical properties, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM D638
Flexural Strength 135 MPa
19600 psi
Flexural Modulus 5.00 GPa
725 ksi
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
ASTM D648
Flammability, UL94 V-0
V-0