Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unipetrol PE HD LITEN® MB/ML 72 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Unipetrol RPA
Trade Name PE HD LITEN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol PE HD LITEN® MB/ML 72 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Made for injection molding applications.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ISO 1183
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ISO 306