| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
| Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 250 °C |
15 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 87 | 87 | 30S reading; ASTM D2240 |
| Tensile Strength at Break | 18.0 MPa | 2610 psi | Type I, 50 mm/min; ASTM D638 |
| 18.0 MPa | 2610 psi | 50 mm/min; ISO 527 | |
| 27.0 MPa | 3920 psi | after 7days @136°C; UL 1581 | |
| 30.0 MPa | 4350 psi | UL 1581 | |
| Elongation at Break | 130 % | 130 % | 50 mm/min; ISO 527 |
| 140 % | 140 % | Type I, 50 mm/min; ASTM D638 | |
| 200 % | 200 % | after 7days @136°C; UL 1581 | |
| 280 % | 280 % | UL 1581 | |
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
| 0.100 GPa | 14.5 ksi | 12.5 mm/min; ISO 178 | |
| Heat Distortion | 20 % @Load 0.250 kg, Temperature 121 °C |
20 % @Load 0.551 lb, Temperature 250 °F |
UL 1581 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL temperature rating; UL 1581 |
| Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
| Oxygen Index | 28 % | 28 % | ISO 4589 |
| Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
| 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.40e+16 ohm-cm | 2.40e+16 ohm-cm | ASTM D257 |
| Dielectric Constant | 2.6 @Frequency 1.00e+6 Hz |
2.6 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dielectric Strength | 28.0 kV/mm @Thickness 1.50 mm |
711 kV/in @Thickness 0.0591 in |
in oil; IEC 60243-1 |
| Dissipation Factor | 0.0028 @Frequency 1.00e+6 Hz |
0.0028 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Smoke Density on 0.5mm plaque, Flame, Ds, max | 143 | ASTM E 662 |
| Smoke Density on 0.5mm plaque, Non-flame, Ds, max | 67 | ASTM E 662 |