| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics NORYL HM3020H PPE+PS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Water Absorption | 0.060 % @Time 86400 sec |
0.060 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0025 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 17.7 g/10 min @Load 2.16 kg, Temperature 300 °C |
17.7 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 88 | 88 | ASTM D785 |
| Tensile Strength, Yield | 115 MPa | 16700 psi | SABIC - Japan Method |
| Elongation at Break | 4.0 - 6.0 % | 4.0 - 6.0 % | SABIC - Japan Method |
| Flexural Strength | 147 MPa | 21300 psi | ASTM D790 |
| Flexural Modulus | 7.94 GPa | 1150 ksi | ASTM D790 |
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 24.0 - 34.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
13.3 - 18.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 1.8 MPa (264 psi) | 125 °C @Thickness 6.40 mm |
257 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |